Hi all,
How does the amount of metol, sodium sulphite, hydroquinone, sodium carbonate, potassium bromide, and sodium hydroxide affect development time?
I ask becuase I'll try Orwo 842 (replacing phenidone with metol) instead of Ilford PQ Universal. They time I used with PQ was at 24 degrees celsius for 10 minutes. I assume this is aprox 14:30 if developed at 20 degrees celsius.
The film developed was Tmax400 (at about 160 ISO) and the time is for first development in reversal processing.
The Orwo recipe is here: http://lostlabours.co.uk/photography/formulae/developers/rev_filmotec.htm
Note that Im intending to use the second developer as first developer (meaning omitting the thiocyanate).
Here is the PQ recipe: http://lostlabours.co.uk/photography/formulae/developers/devID62.htm
(UPDATE: I used the concentrated stock diluted 1:5)
I get that assuming development time isnt an exact science... but I figured Id try 14:30 at 20 degrees celsius as this have given good results with PQ. But, are there components in the Orwo recipe that differs to such an extent from the PQ recipe I should consider reducing or prolonging the development time some?
Cheers
Peter
How does the amount of metol, sodium sulphite, hydroquinone, sodium carbonate, potassium bromide, and sodium hydroxide affect development time?
I ask becuase I'll try Orwo 842 (replacing phenidone with metol) instead of Ilford PQ Universal. They time I used with PQ was at 24 degrees celsius for 10 minutes. I assume this is aprox 14:30 if developed at 20 degrees celsius.
The film developed was Tmax400 (at about 160 ISO) and the time is for first development in reversal processing.
The Orwo recipe is here: http://lostlabours.co.uk/photography/formulae/developers/rev_filmotec.htm
Note that Im intending to use the second developer as first developer (meaning omitting the thiocyanate).
Here is the PQ recipe: http://lostlabours.co.uk/photography/formulae/developers/devID62.htm
(UPDATE: I used the concentrated stock diluted 1:5)
I get that assuming development time isnt an exact science... but I figured Id try 14:30 at 20 degrees celsius as this have given good results with PQ. But, are there components in the Orwo recipe that differs to such an extent from the PQ recipe I should consider reducing or prolonging the development time some?
Cheers
Peter
Last edited: