Hi there, I'm tying to use the zonal system following St. Ansel directions.
The film that I'm using is tri-x 320 and the developer is Hc 110 1-29 for about 7 min at 20°C.
My problem is that I can find the density 0,10 in the zone 1 around when it is exposed at iso 500/640 when I expect it around iso 250.
I've tried two different emulsions and the results are almost the same.
Can anyone help me?
Thanks in advance
gino