I am triying to increase the contrast of my RA-4 prints with "double developing", taking bits of information from here and there in APUG. It has worked rather well but I am obtaining the stains you can see in the next picture:
The yellow one on the far right was formed in front of my eyes when driying.
Prints are develop in a Jobo CPP3 at 35º C and the process is like that:
* Prewash 30 seconds
* Develop - 45 seconds
* Stop (3% acetic acid) - 30 seconds
* Rinse (water) - 30 seconds
* Fixing (regular B/W) - 2 minutes
* Clearing (15 gr/liter sodium sulfite) - 30 seconds
* Rinse (Water) - 2x30 seconds
* Bleach (15 gr/liter potassium ferricyanide) - 45 seconds
* Clearing (15 gr/liter sodium sulfite) - 30 seconds
* Rinse (water) - 2x30 seconds
* Develop - 45 seconds
* Stop (3% acetic acid) - 30 seconds
* Rinse (water) - 30 seconds
* Blix - 45 seconds
* Rinse (water) - 3x30 seconds
Any idea of what it is causing the stains and how to avoid it? Any improvement in the above process is also welcome...
Thanks in advance.

The yellow one on the far right was formed in front of my eyes when driying.
Prints are develop in a Jobo CPP3 at 35º C and the process is like that:
* Prewash 30 seconds
* Develop - 45 seconds
* Stop (3% acetic acid) - 30 seconds
* Rinse (water) - 30 seconds
* Fixing (regular B/W) - 2 minutes
* Clearing (15 gr/liter sodium sulfite) - 30 seconds
* Rinse (Water) - 2x30 seconds
* Bleach (15 gr/liter potassium ferricyanide) - 45 seconds
* Clearing (15 gr/liter sodium sulfite) - 30 seconds
* Rinse (water) - 2x30 seconds
* Develop - 45 seconds
* Stop (3% acetic acid) - 30 seconds
* Rinse (water) - 30 seconds
* Blix - 45 seconds
* Rinse (water) - 3x30 seconds
Any idea of what it is causing the stains and how to avoid it? Any improvement in the above process is also welcome...

Thanks in advance.