[TABLE="width: 270"]
Water |
[TD="align: right"]750[/TD]
[TD="align: right"]375[/TD]
Solution A |
[TD="align: right"]100[/TD]
[TD="align: right"]50[/TD]
Solution B |
[TD="align: right"]100[/TD]
[TD="align: right"]50[/TD]
Pin Yellow |
[TD="align: right"]3.5[/TD]
[TD="align: right"]1.75[/TD]
"@1:2000 |
Water to |
[TD="align: right"]1000[/TD]
[TD="align: right"]500[/TD]
[/TABLE]
This is a paste from a very old spreadsheet of collected developer info that I have. I have little memory of any details or sources but it may be a starting point for you. My Pinacryptol Yellow had turned brown before I ever got to experimenting and I never returned to it, so I can't give you any useful hands-on information. My notes showed rather long times for most films with medium speed films needing 16-18 minutes and advice to not overexpose.