wilsonneal
Member
Hello Pyrocat-HD users
I processsed my first 10 sheets of TMY 8x10 in Pyrocat HD yesterday. My exposures were a little erratic as I was dealing with bellows factor and goofed, but I did get a few sheets that were at least in the ballpark at EI 320.
I am not seeing as much stain as I expected. I do see a slight warm, yellowish cast, but not to the degree I anticipated. The only other pyro negs I've ever seen were PMK negs and they had a bit more obvious stain.
I used distilled water for making A and B, and am using 1:1:100 dilution.
Also, regarding fixer. I used the PF TF-4 fixer. My first experience with it. Has a disagreeable ammonia odor. I've read that you should NOT reuse this fixer with Pyro negs, so it's a one shot and dump solution. Is that right? What happens if you reuse it? Is there any other fixer that can be reused?
Thanks
Neal
I processsed my first 10 sheets of TMY 8x10 in Pyrocat HD yesterday. My exposures were a little erratic as I was dealing with bellows factor and goofed, but I did get a few sheets that were at least in the ballpark at EI 320.
I am not seeing as much stain as I expected. I do see a slight warm, yellowish cast, but not to the degree I anticipated. The only other pyro negs I've ever seen were PMK negs and they had a bit more obvious stain.
I used distilled water for making A and B, and am using 1:1:100 dilution.
Also, regarding fixer. I used the PF TF-4 fixer. My first experience with it. Has a disagreeable ammonia odor. I've read that you should NOT reuse this fixer with Pyro negs, so it's a one shot and dump solution. Is that right? What happens if you reuse it? Is there any other fixer that can be reused?
Thanks
Neal