Hey,
I Just developed(dektol 1:10) a roll of 400TX and when rinsing I noticed they had a purple shine on them. From previous experiences with T-Max development I thought the film was unsufficiently fixed, so I tried fixing an extra 3mins, while already fixing for 8mins, but the film seemed to get even more purple.
Anyone got any idea's why the film might be purple and/or how to fix this?
Thanks
I Just developed(dektol 1:10) a roll of 400TX and when rinsing I noticed they had a purple shine on them. From previous experiences with T-Max development I thought the film was unsufficiently fixed, so I tried fixing an extra 3mins, while already fixing for 8mins, but the film seemed to get even more purple.
Anyone got any idea's why the film might be purple and/or how to fix this?
Thanks