Precision cookers and C-41 chemicals....

OP
OP

sperera

Subscriber
Joined
Mar 6, 2009
Messages
607
Location
Gibraltar
Format
Multi Format
I think the Anova precision cooker i have is indeed overkill as I get faster results - Ive been testing all afternoon - filling up a water cooler (as you all suggested!) with hot water off the kitchen tap and immersing the Paterson plastic graduates I have enough to go over the level of the 1000ml or 500ml (2 rolls or 1 roll) inside and just waiting for the developer to get to 38 degrees centigrade and thats it......would take the Blix out at the same time.....Ive developed 6 rolls so far doing it as a variation of this and good results.....
Here's a shoot i developed without the precision cooker and just hot water bath pulling it out and starting development as soon as it hit 38 degrees.....
Dead Link Removed

here's a shot from that link....
 

Chan Tran

Subscriber
Joined
May 10, 2006
Messages
6,843
Location
Sachse, TX
Format
35mm
I don't think the foam is needed. It reduces heat loss but if the heater is powerful, heat loss actually makes the temperature more stable.
 

MattKing

Moderator
Moderator
Joined
Apr 24, 2005
Messages
53,194
Location
Delta, BC Canada
Format
Medium Format
The softer plastic bottles that are lousy for storing chemicals long term are fine for tempering chemicals, and may be easier to keep mostly submerged.
And use an insulated cooler.
Think of the JOBO bottles.
 

Cholentpot

Member
Joined
Oct 26, 2015
Messages
6,748
Format
35mm
I use one of those small foam coolers and 1liter soda bottles. Temps stay where I need them with no issues.
 

trendland

Member
Joined
Mar 16, 2012
Messages
3,398
Format
Medium Format

Ok - that looks realy fine.
Imagine - if you would have made this shot by yourself - it would look more fine....
With regards
 

Ko.Fe.

Member
Joined
Apr 29, 2014
Messages
3,209
Location
MiltON.ONtario
Format
Digital
I'm using plastic container which fits into the sink. I put hot tap water and adding boiling water. It brings my C-41 1L bottles which are stored in refrigerator to the temperate I need quick. While temperature goes up, I shake bottles and monitoring temperature of developer. Once the temperature I need is reached, I do developing and keeping developer bottle in the container with hot water, removing it for agitations.

This is E-6 expired Kodakchrome slide film developed by E-6 at home recently by using of the same method. But I have to add boiling water twice to reach E-6 temperature. Now I know why they say "cooking" instead of developing :

 

Old-N-Feeble

Member
Joined
Feb 22, 2012
Messages
6,805
Location
South Texas
Format
Multi Format
I don't think the foam is needed. It reduces heat loss but if the heater is powerful, heat loss actually makes the temperature more stable.

That may be true if the heater is grossly oversized for the bath but if it's the correct size then the insulation helps stabilize the temperature.
 

rbultman

Member
Joined
Sep 1, 2012
Messages
411
Location
Louisville,
Format
Multi Format
Probably most covered, but I'll add my process anyway. I use the Anova for C-41 with the Jobo 1L wide mouth bottles for the chemicals. I use a tub that is large enough for all of the chem bottles and is high enough such that most of the bottle height is covered by the bath. Works great. You just need to let it run long enough such that the chemicals get to temperature. I chose the wide mouth bottles to allow the most rapid transfer of liquid from the bottle to the development tank. I use the Paterson development tanks.
 
Cookies are required to use this site. You must accept them to continue using the site. Learn more…