timeUnit
Member
I recently shot two rolls of Tri-x at EI 800 (on camera) in my Zeiss Ikon (ZM). Developed in XTOL 1+1 20°C, 10 min 30 sec. 1 min init. agitation, then 10 sec / 1 minute. Fix in Hypam 1+4 5 minutes. Wash using Ilford method.
I printed a few frames yesterday and was very surprised to find such fine grain! Print size was 24x30 cm (9.5 x 12 inches). The grain is MUCH finer than I got from HP5+ at EI 400, developing in XTOL.
As I try to avoid Kodak and support Ilford, I'm a bit miffed about these results. Might they be from a shortish developing time? The negs are a bit soft.
On the other hand, the grain I get from HP5+ is very nice, and I miss it a little.
It's been a while since I shot HP5+ in 135-format, and my shooting/developing technique has improved, so the results I'm comparing with might be less than stellar.
Anyone having similar or different experiences with Tri-X and HP5?
Thanks!
Henning
I printed a few frames yesterday and was very surprised to find such fine grain! Print size was 24x30 cm (9.5 x 12 inches). The grain is MUCH finer than I got from HP5+ at EI 400, developing in XTOL.
As I try to avoid Kodak and support Ilford, I'm a bit miffed about these results. Might they be from a shortish developing time? The negs are a bit soft.
On the other hand, the grain I get from HP5+ is very nice, and I miss it a little.

Anyone having similar or different experiences with Tri-X and HP5?
Thanks!
Henning