- Joined
- Apr 9, 2011
- Messages
- 86
- Format
- 35mm RF
Hello,
After looking at YouTube I came up with the following steps to develop my Adox CMS 20 film, my first attempt at developing film. All the working solution will be at 20C but my washing water will be at 28C. Can someone help verify if my steps below are correct
1. Developer fluid (adotech) agitate first 30s then 5s of every 30s thereafter for five minutes.
2. Pour in stop bath (eco-pro acid stop bath) and agitate continuously for 30s.
3. Pour in rapid fixer (premium Arista) and agitate the first minute and leave it for one minute.
4. Rinse first wash with water continuously for 5minutes
5. Immerse in Eco-pro hypo wash for 5 minutes agitating it for the first half of the time.
6. Final wash with water for 10minutes
7. Immerse in wetting agent for 30s without agitating
8. Hang to dry
Thanks
Mark
After looking at YouTube I came up with the following steps to develop my Adox CMS 20 film, my first attempt at developing film. All the working solution will be at 20C but my washing water will be at 28C. Can someone help verify if my steps below are correct
1. Developer fluid (adotech) agitate first 30s then 5s of every 30s thereafter for five minutes.
2. Pour in stop bath (eco-pro acid stop bath) and agitate continuously for 30s.
3. Pour in rapid fixer (premium Arista) and agitate the first minute and leave it for one minute.
4. Rinse first wash with water continuously for 5minutes
5. Immerse in Eco-pro hypo wash for 5 minutes agitating it for the first half of the time.
6. Final wash with water for 10minutes
7. Immerse in wetting agent for 30s without agitating
8. Hang to dry
Thanks
Mark
)