I'm developing a single quarter plate 3.25x4.25(of homemade emulsion) in pmk 1:2:100 in a 5x7 tray. 200ml's of developer is sufficient to cover the plate in that tray.
Is that enough developer to properly develop the plate? Will my sodium thiosulfate bath mixed 30g:200ml be enough to properly fix the plate?
I feel kinda silly asking this, but i've always used rapid fixer and never developed a single sheet by itself
Is that enough developer to properly develop the plate? Will my sodium thiosulfate bath mixed 30g:200ml be enough to properly fix the plate?