Yesterday, I tried lith printing for the first time. These are from the same negative, but on different papers (the first is Foma Variant, the second an Agfa RC). 30 minute development for each.
In the winter, it's hard to maintain temp. in my darkroom. Since I'm making small (5x7 & 8x10) prints, until I get a better handle on the possibilities, I'm putting the developer into a hot water bath between prints, and floating the small tray in a larger tray filled with hot water. Still, the temperature drops significantly over the 30 minutes.
I'm going to try it again today. I now have "old brown". Any suggestions for it's use? Also, any recommendations on shortening the development times?
Thanks.
In the winter, it's hard to maintain temp. in my darkroom. Since I'm making small (5x7 & 8x10) prints, until I get a better handle on the possibilities, I'm putting the developer into a hot water bath between prints, and floating the small tray in a larger tray filled with hot water. Still, the temperature drops significantly over the 30 minutes.
I'm going to try it again today. I now have "old brown". Any suggestions for it's use? Also, any recommendations on shortening the development times?
Thanks.