Steve;
There are formulas out there that do not need ammonia.
In addition, you can take an ammonia type formula and use the acid base cycle (ammonium sulfate), or you can add the iodide at the end of the make, you just have to add less or you will fog the emulsion.
PE
Well, making ammonia shouldn't be too bad. I ordered loads of laboratory glassware and stuff and set up the equipment I needed (nice and cheap off eBay) and waited for the chemicals to arrive (marble chips, Ammonium Chloride, that sort of thing...)
And waited...
And waited...
Most the people on eBay have been great, but the one guy I ordered the chems from is either a bad apple or, if his excuses are to be believed, eBay screwed up.
I'm still hopeful I may get the stuff eventually...
Meanwhile I tried making CaO from 'precipitated chalk' which I am assured is ground limestone.
Either I was assured incorrectly or the brewery supplier who supllied me didn't give me precipitated chalk at all, but gypsum or possibly magnesium carbonate rather than calcium carbonate...
Either way, I must have put enough heat into it to weld a battle ship (cracking the crucible in the process) and the stuff was just the same as when I started, but warmer...
Anyway, I will master it - I'm determined!
I went for a walk through an ancient quarry at the weekend and managed to pick up some lumps of what I think are limestone. I knocked off a few chips with a hammer and put a blow torch on them for a few minutes and, after they cooled, put them in water where they fizzed reasuringly, giving me a white milky solution. So, now all I've got to do is get the barbeque REALLY hot
OK, this is getting a bit silly. At this rate I will be sourcing the gelatine by buying my own cow
But, its kinda fun, just not sure what it has got to do with photography!
Steve