If you're getting spots near frame 17, then I'm assuming that's the top loop on the hanger where bubbles can accumulate and cause marks if not properly agitated. It's possible your delay is too long.
Generally the nitrogen gas burst should be 2" every 10" ( raising the solution level by around an inch ).
Gas should ideally go through a humidifier before feeding the tank.
Stabiliser tank can be tricky to get right. Concentration balance is vital.
You may also look into installing a 'wet trough' in the drying cabinet to add some humidity.
John S