So, lately I got chalk on my negatives because our water softener is broken and I decided to get some purified water to develop in so I don't get stains. But what's happening instead is I get lots more stains then I would have with my hard water ..... I really don't know whats wrong. I developed 100 negatives over last two years on the same way and never had an issue...
See the picture. I wash for 10 minutes, then 1 minute photoflo 1-2ml depends on 300-500ml tank size. Then I hang them to dry, wipe of with my fingers (always did this, never an issue) and then I scan / print them. I attached a scan of the problem. It's always happening at the sides of the negatives, never in the middle.
I can wipe it of with a cloth... but it only gets less visible. Cannot wipe it off completely. Seem to have dryed in the neg. What could be the problem?
See the picture. I wash for 10 minutes, then 1 minute photoflo 1-2ml depends on 300-500ml tank size. Then I hang them to dry, wipe of with my fingers (always did this, never an issue) and then I scan / print them. I attached a scan of the problem. It's always happening at the sides of the negatives, never in the middle.
I can wipe it of with a cloth... but it only gets less visible. Cannot wipe it off completely. Seem to have dryed in the neg. What could be the problem?