I have tried everything.. EI 50, 100, 150. Doubling the amount of 'A', splitting the developer into two batches (the latter being mixed right before being poured in).Reducing development time by 20%. Increasing development time. I've tried developing in trays.. I've even gone back to D76.. No matter what I do, I can not get a 'thick' negative. I mean, they are all thin. Printable on silver gelatin but for carbon, it's just not cutting it.I know i'm an idiot for trying to use WD2D+ in a continuous agitation setup, (should have gone with Pyrocat-MC or Rollo Pyro or some other magic juice)Is this film just 'thin'? I need some density! Sorry for the elementary and confusing question. I've been out of this for a few years.