I have some streaks on my negs at the top edge -see scanned image. I don't think it's light leakage as it does not happen with FP4 or Silvermax. My process is as follows:
Wash negatives in Paterson tank
Put in Rodinal at 100:1 dilution - Tank calls for 375 mls for one spool so 3.75 mls Rodinal added
Tank has two spools to prevent the lower one with the film riding up during agitation
Chemicals at 20.C
Agitate for first minute
Stand for 59 minutes
Stop bath
Fix for 5 minutes agitating every minute
Wash 10 minutes
Any clues about causes would be very gratefully received. I have used this process without getting theses streaks for several months. I wonder whether it is bromide drag?
Wash negatives in Paterson tank
Put in Rodinal at 100:1 dilution - Tank calls for 375 mls for one spool so 3.75 mls Rodinal added
Tank has two spools to prevent the lower one with the film riding up during agitation
Chemicals at 20.C
Agitate for first minute
Stand for 59 minutes
Stop bath
Fix for 5 minutes agitating every minute
Wash 10 minutes
Any clues about causes would be very gratefully received. I have used this process without getting theses streaks for several months. I wonder whether it is bromide drag?