I have some pyrocat hd coming from PF. I have quite a number of rolls of tmy-2 to develop. I'll be developing them four at a time in a Jobo 1500 series tank with a capacity of 1 liter. I also plan on using minimal agitation. Could someone who has used this film/developer give me an idea of what time/temp they use? Responses greatly appreciated. This is my first post here. Just a great source of info by passionate people.
I use 12 minutes @ 26ºC, 50 r.p.m for TMY-2. Test first though with a couple of unimportant rolls. I give a 2 minute pre-soak with Jobo processing, as I experienced odd contrast results without the pre-soak.