Does anyone have experience developing Kodak Technical Pan (120 and 4x5) in PMK Pyro?
Just looking for some starting points. I will obviously do some testing, but if anyone has any pointers re time and temperature, they would be greatly appreciated.
No experience with TP in PMK, but I have developed it in 510-Pyro as follows: EI 25, 1:300 dilution, 20 mins @ 70F, continuous agitation for the first minute, then 15 secs agitation at the 10 min mark (semi-stand.) I've never tried a more normal agitation regime, but, if I was so inclined, I'd try 10 secs each minute and develop for 16 mins.