I think that the percentage figures are rough numbers. Unless you do your own tests, everything is a rough approximation. I suggest that you use development times that are easy to remember and intuitive, e.g. times like 4 minutes, 5.8 minutes, 8 minutes, 11 minutes.
I did TMAX 100 4x5 testing with TMAX 100 developer using the BTZS process with the results measured by the View Camera Store. My results in BTZS tubes at 75 degrees differed quite a bit from published numbers but seem consistent.
For minus through normal development, I use TMAX RS developer at 1:9 dilution. For plus development I use 1:4 dilution. The processing times range from 4 minutes in dilute developer for minus development to as long as 16 minutes in stronger developer for plus development. I can range from about N-2 to N+2.
Don't forget that film speed changes with development, in my case by a considerable degree. Film speed is slower with contracted development and higher with expanded development.