As I have stated in previous posts, I get identical results (uniform development, no streaking) using the following development methods:
1. Stand and Semi-Stand developing of 4x5, 5x7 and 8x10 sheet film in slosher trays developed in Pyrocat-HD, Pyrocat-P and Pyrocat-MC. Film emulsion facing up, with 5 minute tempered water pre-soak.
2. Stand and Semi-Stand developing of 4x5, 5x7 and 8x10 sheet film in BZTS type tubes (i.e., tube in vertical orientation), developed in Pyrocat-HD, Pyrocat-P and Pyrocat-MC. with 5 minute tempered water pre-soak.
See
there was a url link here which no longer exists)