Ian
You are right I should have checked my notes before mentioning Agfa but I was in a hurry and didn't want to dig them out.
However from my freshly dug out notes --
Agfa recommended a 2% solution of anhydrous sodium carbonate. For single and double weight papers, wash the prints for 10 minutes. Then soak the prints for 10 minutes in the working solution with frequent agitation. Finally, wash the prints for an additional 5 minutes. Useful capacity is 100 8x10 prints per gallon of working solution. In any case, the used working solution should be discarded after 24 hours.