Harden those tintypes

kevin klein

Member
Joined
Mar 20, 2006
Messages
194
Format
Large Format
It has come to my attention this past month that the dry tintype must be hardened befor development in the Dektol/thyocyanate developer.

Below you can find an exhample of what can happen without hardening. (.5 gm alum: to 1 oz. water. harden 1 min.)

Using developer D-19(dev 3 min) with cyanate requires no hardening but the plate is not as bright.
 

Attachments

  • kevhouse.jpg
    48.6 KB · Views: 157