• Welcome to Photrio!
    Registration is fast and free. Join today to unlock search, see fewer ads, and access all forum features.
    Click here to sign up

Forte Polywarmtone yellowing

spanish market

A
spanish market

  • 0
  • 0
  • 10
Paper Birch.jpg

H
Paper Birch.jpg

  • 0
  • 0
  • 23

Recent Classifieds

Forum statistics

Threads
203,059
Messages
2,849,285
Members
101,627
Latest member
GeorgeGGV
Recent bookmarks
1

Gary Holliday

Subscriber
Joined
Apr 12, 2006
Messages
827
Location
Cambridge, UK
Format
Medium Format
I've just finished a series of prints on Forte Polywarmtone FB in Ilford Warmtone developer.

After reviewing them, I've noticed that 3 of the prints have very strong yellowing on the image and borders.

As I tend to experiment a lot, I gave some of the prints 1.5 - 2 mins underdevelopment during the session to achieve a warmer look. The other prints were given 4 minutes.

All prints were soaked overnight, washed in running water, hypo cleared and washed again for 10- 15 mins in running water.

Is this yellowing normal with over exposing and under developing? Or has there been a problem with the fix or washing?

Thanks.
 
Last edited by a moderator:
This kind of yellowing is incomplete fixing, you really need to use 2 bath fixing ensuring the silver-thiosulphate complexes are totally soluble and wash out.

Ian
 
Forte polywarmtone needs fresh, strong (film strength) fixer.
 
I agree with Ian and Andreas regarding fresh fixer.

Note: Forte PWT is one of my papers of choice, and it responds most beautifully when using developers that include Glycin. It gets rid of the greenish cast.

Regards,
Paul
 
Last edited by a moderator:
i would suggest that the ratio of fixer is too weak. switch to 1:3
 
It's not so much the strength of the fixer it's more the silver content, so as you used a one bath fixer the silver content builds up, as a consequence the residual silver-thiosulphate complexes aren't fully soluble in water.

Ian
 
Last edited by a moderator:
i would agree that it is the silver content; and frankly i count prints when i print for archival purposes (meaning surface area).

with test prints i might use 1:9, but not for any serious work.
 
Ian, it's not only silver content with polywarmtone. I had this happen with two bath fixing and rather old, but low silver content second bath. It seems to be more complex.
 
this can occur with any paper, not just the polywarmtone.
 
I heard it was a great paper. There is a camera store that has a few 11x14 50 sheet packs left...I was wondering if I should try it out.
 
This seems to happen more with Warm-tone papers than other.

Ian, it's not only silver content with polywarmtone. I had this happen with two bath fixing and rather old, but low silver content second bath. It seems to be more complex.

I'd never really thought about it but it never happened at all when I first started in photography using Bromesko or Kodak Bromide paper, fixing in Sodium Thiosulphate fixers. Then using Ilford Galerie, Multigrade never a problem.

As soon as I began using Record Rapid (Portriga) and by then only Ammonium Thiosulphateb fixers, 1985/6 fixing became more of an issue, that continued with Multi-Contrast Classic. (It's never an issue with RC papers). Forte Polywarmtone seems more susceptible, it's a thicker paper base.

Some people fix in Ammonium Thiosulphate fixers and then use a plain Sodium Thiosulphate bath prior to washing, that seems to make a lot of sense.

Ian
 
I had it happen with polywarmtone RC. While I agree, that proper fixing is not trivial with all papers, polywamtone seems to be extra picky.
 
What shop? I'd be very interested in purchasing it.

Try B&H, they to have some in stock, look for "Polygrade Warm Plus - same stuff I believe - if you click on "more info", Polywarmtone is described as the product, or as the old version of the same . I'm not absolutely sure, so check it out and judge for yourself.
 
Last edited by a moderator:
Some people fix in Ammonium Thiosulphate fixers and
then use a plain Sodium Thiosulphate bath prior to
washing, that seems to make a lot of sense. Ian

May make a lot of sense but not so much more than
other methods as posts this thread will verify. Ansel
did use a 'Plain fixer" made alkaline with sodium
sulfite prior to toning with KRST in a solution
of Kodak HCA.

Of course there is always the question of what is the
sensible thing to do and what are the priorities.
Sensible being an observance of the priorities.

I'd say the usual top priority is convenience.
Repeatedly pouring fixer in and out of a bottle and
tracking the square inches processed is convenient
for some. It ignores though the actual condition of the
used fixer. The condition of the fixer should be the top
priority. Counting square inches is a one-size fits all
papers approach which can lead to wide margins
for error and good chemistry down the drain.

With the condition of the fixer as the top priority
it's proof of doing well is the print it self. My method
establishes a chemistry minimum for each paper. What
ever the dilution happens to be using a standardized
processing technique I'm assured of a thoroughly
fixed print with little margin of chemistry
going down the drain. Dan
 
Photrio.com contains affiliate links to products. We may receive a commission for purchases made through these links.
To read our full affiliate disclosure statement please click Here.

PHOTRIO PARTNERS EQUALLY FUNDING OUR COMMUNITY:



Ilford ADOX Freestyle Photographic Stearman Press Weldon Color Lab Blue Moon Camera & Machine
Top Bottom