I don't see why not. From what I understand, it is actually just concentrated FG-7,with maybe a little sodium sulfite tossed in for good measure. I used to use it with Tmax 100 and really liked it. Since they don't seem to make it anymore, you may have a hard time finding dev time/temp info for it, but no reason why it wouldn't also be good with the Delta films from Ilford, or even traditional films like FP4+ or Tri-X. Burn a roll that you don't care about subject wise and develop it and find out.