Having failed in the past to use potassium permanganate to process Tri-X 7266 and Fomapan R100, I've been using potassium dichromate + sulphuric acid instead with great results. The biggest drawback for me is the toxicity of dichromate; I just feel really uncomfortable using this stuff. Which leads me to give permanganate another go PLUS sulphuric acid as suggested by ILFORD. I didn't add sulphuric acid in the past.
http://www.ilfordphoto.com/Webfiles/20061291034093.pdf
A friend said it works great with Tri-X, but doesn't know if this will work with Fomapan R100 or ORWO UN 54.
Anyone have any experience with the permanganate recipe with Fomapan or ORWO UN 54?
http://www.ilfordphoto.com/Webfiles/20061291034093.pdf
A friend said it works great with Tri-X, but doesn't know if this will work with Fomapan R100 or ORWO UN 54.
Anyone have any experience with the permanganate recipe with Fomapan or ORWO UN 54?
there was a url link here which no longer exists), I store mixed permanganate bleach, in "high" concentration ( 50g KMn04 /L - according Lawless article), in a well stopped brown bottle, since weeks. Even what I called "stage I" dilution (the above 1+9, 5g/L) seems to keep long, the same way.