I recently posted a question regarding my bad negs. I took an example back to my source and it was decided my chemicals or technique was not at fault. My unused film was replaced with a new batch and i have just uploaded two examples of the new film. Apparently the bad film did not stain in an even manner? Probably the film would have been ok for other types of developers.
 