I posted this on Reddit but with little luck, hopefully there’s more insight on here.
C41 streaking problem - help
I’ve developed 10ish rolls of C41 since I started learning in October, on most rolls I’ve gotten these strange streaks. Here’s my most recent example...
It’s quite bad as you can see.
But I do everything by the book! The book being this Kodak Publication (https://125px.com/docs/techpubs/kodak/cis211-Flexicolor_in_small_tank.pdf) on doing C-41 at home with a small tank. Albeit, I use Tetenal chemistry, but I use this method since Tetenal outlines no instructions for small tanks.
In this case, all chemicals were mixed yesterday with deionised water and sat in a Sous Vide controlled water bath until chemicals were heated to 38°.
5 min presoak (38°)
3:15 min development, 30 sec initial agitation, followed by 2 sec of agitation every 15 secs.
6:30 min Bliz. 30 sec initial agitation, followed by 5 sec of agitation every 15 secs. I diverted from Tetenal’s instructions here, only because I thought these streaks were maybe due to under-fixing.
3-4ish rinse. I take the light tight lid part of the Paterson tank to do this part, washing the film directly since at first I thought the wash stage was the problem. I previously just kept that part on and let the water get in that way. I also dunk the reel into a Water/Photo-Flo solution for a minute, lightly agitating.
1 min Stab. I agitate for 30 secs then let it sit.
I then leave to dry, hanging vertically, squeegeeing them with wet fingers a couple of times.
I would really appreciate any insight into this problem, and - if possible- any remedies for this roll? This streaking problem has been driving me nuts for months! Admittedly, it’s also put me off doing C-41 at home all together. But I’m sure many of you don’t get this problem so there must be a way!!
C41 streaking problem - help
I’ve developed 10ish rolls of C41 since I started learning in October, on most rolls I’ve gotten these strange streaks. Here’s my most recent example...
It’s quite bad as you can see.
But I do everything by the book! The book being this Kodak Publication (https://125px.com/docs/techpubs/kodak/cis211-Flexicolor_in_small_tank.pdf) on doing C-41 at home with a small tank. Albeit, I use Tetenal chemistry, but I use this method since Tetenal outlines no instructions for small tanks.
In this case, all chemicals were mixed yesterday with deionised water and sat in a Sous Vide controlled water bath until chemicals were heated to 38°.
5 min presoak (38°)
3:15 min development, 30 sec initial agitation, followed by 2 sec of agitation every 15 secs.
6:30 min Bliz. 30 sec initial agitation, followed by 5 sec of agitation every 15 secs. I diverted from Tetenal’s instructions here, only because I thought these streaks were maybe due to under-fixing.
3-4ish rinse. I take the light tight lid part of the Paterson tank to do this part, washing the film directly since at first I thought the wash stage was the problem. I previously just kept that part on and let the water get in that way. I also dunk the reel into a Water/Photo-Flo solution for a minute, lightly agitating.
1 min Stab. I agitate for 30 secs then let it sit.
I then leave to dry, hanging vertically, squeegeeing them with wet fingers a couple of times.
I would really appreciate any insight into this problem, and - if possible- any remedies for this roll? This streaking problem has been driving me nuts for months! Admittedly, it’s also put me off doing C-41 at home all together. But I’m sure many of you don’t get this problem so there must be a way!!