Bruce (Camclicker) said:
The prints will be enlargements of 4X5 negs.; VC Silver Fiber (MG Warmtone); the Jobo is CPE 2 with lift.
Thank you again (and again), you are really helpful. I'm sure your "fairly good data" is better than any I could drum up.
Bruce,
Use the 1:1:100 dilution of Pyrocat-HD at 72º F. Develop with rotary agitation (slow) for the following times.
SBR 9 (N -0.5) 6:00 minutes
SBR 7 (N) 9:30 minutes
SBR 6 (N+0.5) 15:00 minutes
This should get you into the ballpark, but test carefully with your own equipment and materials.
Best,
Sandy