You may have over-developed it a bit.... Of course, I am looking at scanned result so I'm not certain. I typically use D-76 so I can't share my experiences.
22 minutes will be about 50% over developed in Pyrocat HD at that dilution & temperature, the times for most films except Foma are aound the 15 minute mark. Foma require less about 10-12 minutes or the contrast goes to high.
Thanks for answers!
The resume - for a film 400 iso 1+1+100, 20C, 12-15 minutes
For 100 and 200 iso 10-12 minutes.
Correctly?
And how to be with films 800 iso and above?
Push process is possible?