troutmask
Member
Anybody using this paper? I have run a search here but couldn't find anything.
I have some and ran a couple of tests today.
In Ilford warmtone developer 1:9 at 24 dgrees (college darkroom, water is always this warm)
MDT above 3 below 4 mins, havn't broken it down any further.
Flash test (using RH designs paper flash 4 secs + 1/10 stop
Anybody else who has tested the paper i would be interested in haring as a poor studnt I have to save paper! Dry down % would be useful to know as I assume this is not affected by developer etc. but is a constant?
I am making assumtions here but am I right in thinking that both the MDT and the flash tim would be longer in Ilford Cooltone? Or would the devloper used only affect the MDT?
I have some and ran a couple of tests today.
In Ilford warmtone developer 1:9 at 24 dgrees (college darkroom, water is always this warm)
MDT above 3 below 4 mins, havn't broken it down any further.
Flash test (using RH designs paper flash 4 secs + 1/10 stop
Anybody else who has tested the paper i would be interested in haring as a poor studnt I have to save paper! Dry down % would be useful to know as I assume this is not affected by developer etc. but is a constant?
I am making assumtions here but am I right in thinking that both the MDT and the flash tim would be longer in Ilford Cooltone? Or would the devloper used only affect the MDT?