I developed a rollfilm with pyrocat HD as a 2 bath. 1:20 5minutes in A and 10 minutes in B. This is the result.
Light values measured are entered in EV
Thats really neat Willie Jan,I have close to the same situation as you have in your photograph here. I was thinking of using a high dilution of hc110 1:100 or more but have my doubt's ,have heard that pryo works good for this kind of development. Now that I see your photograph I think I'll give pryo a try,it has worked very good on your photo. Thanks for the example.