djkloss
Subscriber
I developed two rolls of Tmax 100 in HC110 dilution B at 70 degrees and they came out mottled. Is that due to HC110 being 'high energy'?
Thanks.....
Dorothy
Thanks.....
Dorothy
MattKing said:The almost looks like reticulation. What was the temperature of the pre-wet, water stop, fixer, and wash?
Not enough temperature difference to be a factor.djkloss said:Temp was 70, to start. It may have gradually dropped for each step after that. The final wash was 68
djkloss said:thanks. I think I'll go back to rodinal and silver based films. never did like tmax anyway.
Tom Hoskinson said:The image you posted is very pixilated and that makes it difficult to judge, but it looks overdeveloped to me.
If you diluted the HC110 with either high pH water or hot water (or both), that could give your working developer a significant activity boost.