Donsta
Member
- Joined
- Jun 11, 2004
- Messages
- 191
- Format
- Multi Format
Following some prints which I could not clear in EDTA (basically anything I develop with potassium oxalate will not clear in EDTA nor an EDTA sodium sulphite mixture), I tried some Heico permawash. It seems to work really well and is dirt cheap - are there any issues I need to consider before making it my standard clearing agent?