thuggins
Member
I just mixed the fifth (final) batch of Tetenal. The first dev and color dev had been decanted into smaller bottles but the blix and stabilizer were in the original 500ml bottles. Part 2 of the blix had formed a yellowish film where it filled the bottom of the bottle, I assume it had oxidized. I saw no indication of this on the previous batch mixed about five weeks ago. I've developed a roll of Velvia 50 and it looks fine.
What does part 2 do, and what is the worse case if some portion of it has oxidized?