maarten m
Member
I just developed a roll of 320TXP (Lc29 1:30, and ilfostop ilfofix) and there's quite a blue appearance on the negatives.
1st step: rinse with water
2nd step: develop LC29 (1:30) (freshly created)
3rd step: stop bath (re-use)
4th step: fixer (re-use)
5th step: rinse (4 10 20 20 wetting agent)
I suspect that stop and fixer are in for replacement due to contamination, though only 5 rolls have been developed in it, while 10 to 15 should be possible. I'm considering to make an extra rince between development and stop bath and between stop- and fixer. anyone have experience with extra rinces between baths?
suggestions?
maarten.
1st step: rinse with water
2nd step: develop LC29 (1:30) (freshly created)
3rd step: stop bath (re-use)
4th step: fixer (re-use)
5th step: rinse (4 10 20 20 wetting agent)
I suspect that stop and fixer are in for replacement due to contamination, though only 5 rolls have been developed in it, while 10 to 15 should be possible. I'm considering to make an extra rince between development and stop bath and between stop- and fixer. anyone have experience with extra rinces between baths?
suggestions?
maarten.